Development of High Chromium White Cast Iron Liquefaction Technology

Main Article Content

Saidmakhamadov Nosir
Karimov Bokhodir
Hudoykulov Shohruh
Bekjanova Laylo

Abstract

In this paper, high-chromium 280X29NL cast iron is reduced to 28.86 – 31% to 14 – 15%, 1% gchach Cu is added, the chemical composition is changed and the new brand 280X15TDL alloy is economically cheap and brittle, without reducing the mechanical properties of the alloy 0.4 was liquefied in an induction furnace. For thermal treatment of the alloy, they were heated to a certain temperature by SNOL – 7.2 / 1100 muffle furnace and cooled in air after standing for a certain time at a temperature of 8500 C. In this process, the chemical composition of the alloy did not change, but its properties changed due to changes in its structure.

Article Details

How to Cite
Saidmakhamadov Nosir, Karimov Bokhodir, Hudoykulov Shohruh, & Bekjanova Laylo. (2022). Development of High Chromium White Cast Iron Liquefaction Technology. Eurasian Journal of Engineering and Technology, 4, 123–127. Retrieved from https://geniusjournals.org/index.php/ejet/article/view/912
Section
Articles

Most read articles by the same author(s)